Voltage Class 6kV~15kV ideal for external insulation and protection of power cable termination and joint
Electrical stress control heat shrinkable tubing made of radiation cross-linked polyolefin for application in power cable termination and Joint
Applications
 For elecIrcal stress control of power cable
termination and joint
Featums/Beneflts
 Specially designed to control high electrical stress
Colour£º Black
Temperature Range
 Operating Temperature: -55~105¡æ
 Shrink Temperature: 120~130¡æ
| Test Item |
Test Method |
Typical value |
| Tensile strength |
ASTM D2671 |
¡Ý11mPa |
| Break out elongation |
ASTM D2671 |
¡Ý300©‡ |
| Low temperature flexibility |
-40¡æ/4hrs |
No cracking |
| Volume resistance |
IEC93 |
¡Ý1010¦¸.cm |
| Dielectric constant |
IEC 60250 |
¡Ý15 |
| Product Code |
thicknessafter free recovery(mm) |
Standard package(m/pcs) |
Standard package(m/roll) |
| C102-16/8 |
1.8 |
1.22 |
15 |
| C102-20/10 |
1.8 |
1.22 |
15 |
| C102-26/12 |
2.4 |
1.22 |
15 |
| C102-30/15 |
2.7 |
1.22 |
15 |
| C102-45/20 |
3.0 |
1.22 |
15 |
| C102-50/25 |
3.3 |
1.22 |
15 |
| C102-65/30 |
3.3 |
1.22 |
15 |
| C102-95/45 |
3.6 |
1.22 |
15 | |
|